I need a product recommendation for a slab-on-ground surface sealer. The product must give a hydraulic conductivity of less than 1x10^-7 cent/sec. The slab is also subject to forklift truck traffic. Any suggestions would be appreciated.
 
Replies continue below

Recommended for you

Lapidolith and Ashford Formula are both routinely used for such applications. As with JAE, I don't know about their hydraulic conductivity, since vapor migration through the slab is not measured in such units.

Both work in a similar fashion as a hardener and sealer. Both work on a chemical ion exchange with calcium in the cement, creating a more dense, less permeable surface. Lapidolith is a magnesium silicate material, whereas Ashford is a sodium silicate material.

Keep in mind that hardener/sealer materials will create a slipper floor because of the closed texture and density at the surface. You might want to consider a slight etch after placement, but be careful that you don't remove all of the material. You can also etch prior to the placement, but consider that etching will reduce the amount of calcium available at the surface, thus could reduce the effectiveness of the material.

Paint on type clear or pigmented "sealers" don't work well for forklift traffic.
 
Status