What section in the ASME Code would I find the Chemical Composition requirments for 5454 Aluminum?
 
Replies continue below

Recommended for you

Thank you very much. I am new to ASME.
 
Extracted From ASME Section II SB-209


Alloy Silicon Iron Copper Manganese Magnesium Chromium Zinc Titanium Aluminum
5454 0.25 0.40 0.10 0.50–1.0 2.4–3.0 0.05–0.20 0.25 0.20 remainder
 