This is a wheel bushing, 6mm OD 316 SS shaft, this bushing (6.5mm ID 10mm OD 30.5mm L), 10.5mm ID PP molded wheel. Load is expected to be ~400N maximum. Maximum speed is <450rpm.
I looked to IGUS, they only make 6mm L standard, so Im using 5x for each wheel which is more money than the brass piece I think.
Thanks still,
Alex