I have a customer requesting us to modify a procedure so that it will be good for 3/8" with impacts. The code is NACE MR0175 and ASME Section IX. Do I need to only weld up a 3/8" plate following the original procedure and have that plate impact tested or does it need to include tensiles/bends/hardness survey and charpy?
I talked to a few people and they each said something different. One says just do the 3/8 plate and do impacts. Another says impacts and hardness survey, while yet another says impacts, hardness, and tensiles.
I talked to a few people and they each said something different. One says just do the 3/8 plate and do impacts. Another says impacts and hardness survey, while yet another says impacts, hardness, and tensiles.