Does anyone have any experience with obtaining charpy impact results for A320 L7 Bolting of diameter M14?
The largest sub size specimen obtainable is 10mm x 5.0mm but there is only acceptable criteria for 10mm and 7.5mm

How do you obtain the impact results for m14 bolt this way?
 