Chameleon Color Paints

Status
Not open for further replies.

TheTsquare

New member
Joined
Jun 30, 2003
Messages
4
Location
US
Can Anyone tell me how the Chameleon style paints that show one color ant one angle and a different color at a different angle? This process perplexes me. I've thought of using dual color metal flakes but that won't solve the problem, and the commercial vendors think that they're move stars and want top dollor for what should be a relatively simple process.

 
It has microscopic parallel grooves which causes light
interference.


<nbucska@pcperipherals DOT com> subj: eng-tips
read FAQ240-1032
 