Dear all
We have been operating our steam cracker for 5 years and the turnaround was delayed one year due to a plant revamping preparation.
I, as a process engineer, am responsible for the compressor follow-up. Suddenly, in the last two months the first two (of five) stages have been loosing performance with the (aprrox) the same flowrate.
The compression ratio decreased and the temperature ratio increased --> fouling... but..suddenly? not progressive
It has lost 9% efficiency in two months and it continues with decreasing trend. We have an antifouling injection for 4 stages (except the 4th one). The rate was increased twice but without sucess. The suction temperature is quite low (32ºC) compared with the past (for volume optimization).
Other, bigger, problem is exactly in the 4 stage. It is "highly efficient". Suction temperatures are quite low and upstream heat exchanger is water limited due to the low T. Very low RT at this stage. I cannot understand what is happening in these pressure range (10 bar) for this cooling. I have been watching Joule-Thomson efect in a downstream drum LIC but this is not the reason. Amazing behaviour but not understandable. Last time this condenser was oppened (due to very high DP) the fouling, after plant shutdown and HE opening, was very cold, like 2-4ºC.
I am now collecting raw gas lab analysis to check isentropic exponents and to try conclude something more.
What can be happening? Every help...is precious to troubleshoot.
AndreChE
We have been operating our steam cracker for 5 years and the turnaround was delayed one year due to a plant revamping preparation.
I, as a process engineer, am responsible for the compressor follow-up. Suddenly, in the last two months the first two (of five) stages have been loosing performance with the (aprrox) the same flowrate.
The compression ratio decreased and the temperature ratio increased --> fouling... but..suddenly? not progressive
It has lost 9% efficiency in two months and it continues with decreasing trend. We have an antifouling injection for 4 stages (except the 4th one). The rate was increased twice but without sucess. The suction temperature is quite low (32ºC) compared with the past (for volume optimization).
Other, bigger, problem is exactly in the 4 stage. It is "highly efficient". Suction temperatures are quite low and upstream heat exchanger is water limited due to the low T. Very low RT at this stage. I cannot understand what is happening in these pressure range (10 bar) for this cooling. I have been watching Joule-Thomson efect in a downstream drum LIC but this is not the reason. Amazing behaviour but not understandable. Last time this condenser was oppened (due to very high DP) the fouling, after plant shutdown and HE opening, was very cold, like 2-4ºC.
I am now collecting raw gas lab analysis to check isentropic exponents and to try conclude something more.
What can be happening? Every help...is precious to troubleshoot.
AndreChE