Was trying to find out the relationship between sulfate exposure (negligible, moderate, severe, very severe), the water-soluble sulfate (SO4) in soil and the Cement Type. UBC 97 had this information, but have not been able to locate this table in the IBC. Appreciate if you can help in where this informaiton is located in the current code.

Thanks
 
Replies continue below

Recommended for you

I think what you are looking for is in ACI 350.

Mike McCann, PE, SE (WA)


 
I believe what your looking for is in the ACI 318. In ACI 318-11 Table 4.2.1.
 