Apr 27, 2009 #1 bigghassan Nuclear Joined Aug 24, 2004 Messages 16 Location LY Hi all Does anybody have an idea why the CEION flush probe is showing negative metal loss?
Apr 27, 2009 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,950 Location GB Shorting by conductive deposits? Instrumentation calibration? Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
Shorting by conductive deposits? Instrumentation calibration? Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Apr 27, 2009 Thread starter #3 bigghassan Nuclear Joined Aug 24, 2004 Messages 16 Location LY Thanks for reply, Is it a practical to clean the probe and return it back to the system? , if not what is the optimum way to eliminate the negative readings. Upvote 0 Downvote
Thanks for reply, Is it a practical to clean the probe and return it back to the system? , if not what is the optimum way to eliminate the negative readings.