I am looking for correlations between CBR and unconfined compression strength. So far I found:
1. qu = 4.5xCBR (psi-Illinois DOT)
2. qu = 47xCBR (kPa-Japan)
The above equations give results with about 50% difference.
Do you have any other references? Since I am in Japan I may be ending up using equation #2. Just curious to see other correlations.
Thanks !!
1. qu = 4.5xCBR (psi-Illinois DOT)
2. qu = 47xCBR (kPa-Japan)
The above equations give results with about 50% difference.
Do you have any other references? Since I am in Japan I may be ending up using equation #2. Just curious to see other correlations.
Thanks !!