I have equipped a test bed for cavitation experiments using the ASTM G32 configuration with a Branson sonifer cell disrupter mod 450 with exponential horn 1/2"(amplitude 10-65 micron). I'm trying to make a calibration with Ni200 samples in modified and not modified configuration. I have some problems in making the Ni tip vibrate in not modified configuration. The tip dimensions are the same as described in the standard with a thickness of 4mm and a diameter of 13mm to fit the horn. Can you help me? Thank you!
 