If it is really cavitation, you can resolve via :
a. increase the system pressure ( e.g. RO )
b. reduce the fluid temp below the fluid boiling point at the given pressure.
a and/or b above will eliminate the formation of bubbles which later lead to cavitation on the collapse of these bubbles.
Good luck !