We have some 50-taper machines (SNK-machines with in-spec 3500lbs. of pull pressure) that have habitually collected pitting and wear on the holder taper.
It has resulted in regular spindle taper regrinding.
We have been recently evaluating the run-out condition of our holders with a proper check fixture, one holder company recommends replacing tools with .0003 or more run-out.
We had to raise the standard to .0005, which still captured over half of our tool holders, many of the new and unused.
Can anyone accurately regrind these 100s of holders or will they need replaced?
Has anyone else had similar machine spindle / holder wear issues?
It has resulted in regular spindle taper regrinding.
We have been recently evaluating the run-out condition of our holders with a proper check fixture, one holder company recommends replacing tools with .0003 or more run-out.
We had to raise the standard to .0005, which still captured over half of our tool holders, many of the new and unused.
Can anyone accurately regrind these 100s of holders or will they need replaced?
Has anyone else had similar machine spindle / holder wear issues?