Oct 3, 2002 #1 danielsadeh Chemical Joined Oct 3, 2002 Messages 1 Location US I am looking for an acrylic that is totaly clear and can be casted in room temperature. Any ideas? and where can I get it?
I am looking for an acrylic that is totaly clear and can be casted in room temperature. Any ideas? and where can I get it?
Oct 3, 2002 #2 insideman Mechanical Joined Nov 21, 2000 Messages 286 Location US Not exactly acrylic, but easily castable and transparent: CASTOLITE. Available at many plastic supply firms including US PLASTICS. Nice prople to deal with. Upvote 0 Downvote
Not exactly acrylic, but easily castable and transparent: CASTOLITE. Available at many plastic supply firms including US PLASTICS. Nice prople to deal with.