Cast 440C Hardness

Status
Not open for further replies.

jksimco

Industrial
Jun 19, 2012
1
I would like to know wat maxumum hardness can be achieved of Investment Casting 440C
I would like to achieve 55 to 60 HRC but could not achieve higher then 40 HRC.
 
Replies continue below

Recommended for you

Have you oil quenched the parts? If yes,then achieving the desire hardness should not be a problem.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 