Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Casing nominal weight

Status
Not open for further replies.

eltooon

Mechanical
Joined
Apr 4, 2011
Messages
33
Location
US
Could someone please enlighten me why there can be two nominal weights for the same OD and wall thickness?

For example, this is what I found on Tenaris Website.
18 5/8" OD 0.500" Wall casing has nominal weight 99ppf and 100ppf (Screenshot in attachment)



We make a living by what we get; we make a life by what we give.
 
The nominal weight is just a name used to designate the product. The differences could be used to denote different collapse ratings, different applications, or perhaps just rounding issues, it is hard to tell.

Your screenshot did not make it to the post, so I cannot see your example.
 