Hi
I am trying to predict the tensile strength of carbon fiber and glass fiber laminates. I will use the laminate theory and the maximun strength failure theory.
Since this is the first time that I will be working with fiber reinforced composites in my country, El Salvador, I am having a hard time in understanding fabrics.
I will use micromechanics to determine the mechanical properties of the laminae, then, using laminate theory, the generalized hooke's law for orthotropic material and the maximun stress failure theory, I will obtain the required uniaxial tensile stress that causes the first ply failure.
Can someone advice me on the subject. My primary reference has been "introduction to composite materials" Stephen Tsai Thomas Hahn.
In most of the books i have found, the laminate theory is explained for unidirectional, orthotropic materials. Does fabrics behave like orthotropic materials?
Where can i find the mechanical properties of a fabric (warp and fill)?
I will use 3k-135-8h carbon fiber and 7781-3800-f3 glass fiber.
Thanks
I am trying to predict the tensile strength of carbon fiber and glass fiber laminates. I will use the laminate theory and the maximun strength failure theory.
Since this is the first time that I will be working with fiber reinforced composites in my country, El Salvador, I am having a hard time in understanding fabrics.
I will use micromechanics to determine the mechanical properties of the laminae, then, using laminate theory, the generalized hooke's law for orthotropic material and the maximun stress failure theory, I will obtain the required uniaxial tensile stress that causes the first ply failure.
Can someone advice me on the subject. My primary reference has been "introduction to composite materials" Stephen Tsai Thomas Hahn.
In most of the books i have found, the laminate theory is explained for unidirectional, orthotropic materials. Does fabrics behave like orthotropic materials?
Where can i find the mechanical properties of a fabric (warp and fill)?
I will use 3k-135-8h carbon fiber and 7781-3800-f3 glass fiber.
Thanks