Hello, I just read, that students are not allowed to ask questions, but I have to try. My bachelor semestral project is about...how to say it (english is my second language)...vaporizing water from caprolactam solution and making it more concentrated (I have to get some technical dictionary).
My main problem is that I do not have any of thermo-physical properties of caprolactam. I tried to search the web and the best I found is
but it is (of course) not free and for me it is quite expensive. Could you help me with this in some way?At least, is it possible to find such information on the web for free?Thank you in advance. Holubar
 
Matweb provides data on a copolymer:


... it also provides the name of the manufacturer who provided the data. A search and a phone call to their engineering department should provide the properties you need.





Mike Halloran