Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Can you explain what this DCP results shows

Status
Not open for further replies.

occo182001

Civil/Environmental
Joined
Sep 26, 2013
Messages
1
Location
NG
Hello I am a training construction manager and am struggling with the DCP test. Can somebody please explain what I am looking at below and what is the analysis I can take from it. It is a laterite based platform the example is taken from


Test point PR Test point PR
T1 T2
110 120
210 100 140 20
270 60 155 15
290 20 160 5
310 20 165 5
330 20 170 5
345 15 185 15
370 25 200 15
410 40 210 10
425 15 215 5
430 5 230 15
435 5 250 20
440 5 280 30
 