Can someone tell me if a fiberglass tubing can be bored to a larger inner diameter?
 
Certainly. Carbide tooling will last longer.

I assume you don't care about the surface finish. It will be rough, and covered with short fibers and cavities where fibers used to be.



Mike Halloran