I am rebuilding a mixer that´s inside a salt bath inside a reactor. The only material that i have available is the 8 " sch. 80 ASTM A53 Gr. B, I´m worried about graphitizing. It will be working at 400 degrees Celcius constant. It will be used as support for the shaft wich is SS A420.