I have some 1/2" plates there were welded together with 1/4 fillet welds.
I probably should have welded them with 3/8" or 1/2" fillet welds.
Can I put another bead ontop of the initial?
Or is this just not possible.
The material is ASTM A572 Grade 50
I probably should have welded them with 3/8" or 1/2" fillet welds.
Can I put another bead ontop of the initial?
Or is this just not possible.
The material is ASTM A572 Grade 50