Can Forged Bar be used for Heads + Caps ?? 1

Status
Not open for further replies.

Lee2006

Mechanical
Feb 22, 2006
28

Can vessel Heads and Flat Ends be machined from SA182 F316L Forged Bar ?
ASME VIII states that Forged or Hot Rolled Bar can be used up to and including DN100 but Im sure I have seen other ASME vessels which have End Caps machined from up to 8" Bar.
 
Replies continue below

Recommended for you

There is a code case which speaks to this possibility. I do not know the number offhand but there are supplemental testing requirements if bar stock (forged bar is still considered bar) is used for shells, heads, or nozzle necks.

EJL
 
Please remember that not all Jurisdictions accept Code Cases.

Suggest you speak with your AIA prior to use. There is more to this.
 