Jun 18, 2007 #1 TCPhoenix Mechanical Joined Jan 23, 2007 Messages 24 Is anyone familiar with CAN/CSA-G40.21. I need to know how CAN/CSA-G40.21 Grade 300W for channels, angles and plates compares to an A36 designation. Does A36 meet the CAN/CSA-G40.21 Grade 300W requirements?
Is anyone familiar with CAN/CSA-G40.21. I need to know how CAN/CSA-G40.21 Grade 300W for channels, angles and plates compares to an A36 designation. Does A36 meet the CAN/CSA-G40.21 Grade 300W requirements?
Jun 18, 2007 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US Please don't cross post. See thread330-189943 Upvote 0 Downvote
Jun 18, 2007 #3 JoeTank Structural Joined Oct 28, 1999 Messages 1,133 Location US No, A36 will not meet the Grade 300W spec. A36 would be more like Grade 260W. Joe Tank Upvote 0 Downvote