Can A333 always be used to replace A106? 3

Status
Not open for further replies.

Downhand

Industrial
Dec 20, 2009
59
Is it always safe to assume that A333/LF2 can be used as a substitute for A106/A105 and is there any difference in how they are manufactured or does the manufacturer simply take a batch of A106 and charpy test it and if it passes it can now be labelled A333?
 
Replies continue below

Recommended for you

No, do not assume. You need to obtain a copy of both ASTM Specifications and compare them regarding metling practice, HT, properties. inspection and end use.
 
Only real difference that matters is A333/LF2 is impact test to a lower temperature.
In reality its the same material.
Never substitute without owners approval though... always saves a NCR.
 
At temperatures above 650F to 700F, the fine grain material has lowered creep strength and at temperatures above 750 F they are more prone to graphitization than A-106/A-105.

 