In ASME II D SUBPART 3,Fig HA-3(SS304L) how to calcuate Factor B value?

At temp 100Deg,Factor A=0.0011 Cel,S=115MPa

Please explain with calculation process like extrapolation or intrapolation if used?
 
Try interpolation using the values in Table HA-3.
 
lingeshgdvg, based on A = 0.0011, T = 100 C, B is in the 8000 psi (55 MPa) range, just reading the chart.

As metalonis says, you can confirm by numerical interpolation from the Table HA-3, or just get out a ruler.