I am just curious. From the notes in appendix A of b31.3 note 57 states "Conversion of carbides to graphite may occur after prolonged exposure to temperatures over 800 F." Why does Caesar II not give any type of warning or error if I am using A106B pipe with operating temperature at 900F?