A cable can be bend 90 degrees if we allow enough space for bending radius
ie,12*diameter of armoured cable.

My question is whether a cable can bend 45degress or 30 degrees like above
if we allow space for bending radius OR what is the minimum limit of degrees
that a cable can be bend if we allow space for bending radius as needed?

thanx in advance

Abraham
 
Replies continue below

Recommended for you

If you are using the minimum bend radius or larger radius throughout the bend, I do not see a reason to limit the degree of turning. What I do not understands is why you would think there would be a restriction on a small bend angle with the same radius as a larger bend.
 
As long as you obey the bend radius, you are good to go as many 360 degree wraps as you want-so a 270 degree bend, no big deal
 
When pulling a cable one has to check also sidewall bearing pressure.
Sidewall bearing pressure is the radial force exerted on the insulation and jacket of a cable
at a bend point when the cable AS under tension. If sidewall bearing pressure is excessive, the conductor will tend to crush the insulation and jacket at the support point.
See : IEEE Std 525-1992 ch. 10.3.1.3 Maximum allowable sidewall pressure:
“Sidewall pressure, P, is defined as the tension out of a bend expressed in pounds divided by the radius of the bend expressed in feet. The sidewall pressure on a cable can be calculated by the following equations:” … eq.6;7;8;9
For instance for a single cable in conduit:
P=To/r
Where:
P is the sidewall pressure, in lb/ft of radius
To is the tension out of the bend, in pounds
r is the inside radius of bend, in feet

 