Jan 26, 2018 #1 ttquick20 Mechanical Joined Jan 26, 2018 Messages 1 Location US I was hoping to find the modulus of elasticity and the tensile strength for C405. It seems to be a branded name of an alloy used in some baseball bats. I'd appreciate any help.
I was hoping to find the modulus of elasticity and the tensile strength for C405. It seems to be a branded name of an alloy used in some baseball bats. I'd appreciate any help.
Jan 26, 2018 1 #2 btrueblood Mechanical Joined May 26, 2004 Messages 10,034 Location US according to this source, C405 is equivalent to 7055. http://www.bomani.com/BSRI2010/BSRI_2010_Members/softball_articles/BSRI-01_sballoys.html Upvote 0 Downvote
according to this source, C405 is equivalent to 7055. http://www.bomani.com/BSRI2010/BSRI_2010_Members/softball_articles/BSRI-01_sballoys.html
Feb 7, 2018 #3 Metalero Materials Joined Jan 30, 2018 Messages 83 Location MX Young's modulus = 70 GPa for aluminum (1) UTS = 627MPa LT Direction (2) References: (1) https://doi.org/10.1016/j.msea.2007.05.116(2) http://www.matweb.com/search/DataSheet.aspx?MatGUID=8755e9a9df8e4ebf8148593d1d3c4545&ckck=1 Upvote 0 Downvote
Young's modulus = 70 GPa for aluminum (1) UTS = 627MPa LT Direction (2) References: (1) https://doi.org/10.1016/j.msea.2007.05.116(2) http://www.matweb.com/search/DataSheet.aspx?MatGUID=8755e9a9df8e4ebf8148593d1d3c4545&ckck=1