Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

C26000 brass, Heat treating and annealing data sheet?

Status
Not open for further replies.

fastline12

Aerospace
Jan 27, 2011
306
Cannot find much information on this alloy and curious if anyone can share a resource for this material?
 
Replies continue below

Recommended for you

This is the common 70Cu-30Zn cartridge brass and as btrueblood notes, can be softened by annealing but not hardened by heat treating. What are you hoping to accomplish? This will have some bearing on the annealing treatment.
 
We have to form the end of some parts which will cause work hardening of the material and we simply need to anneal the end back to preformed state.

My understand as well was that 26000 could not be heat treated, only work hardened.
 