In a water treatment plant designed for Saudi Arabia we installed a hot deep galvanising tank for potable water storage. This tank has inside a butyl rubber liner.
Now after few months the tank has some leaks.
I don't know if this leaks are caused by the free chlorine in the potable water that can oxidize the butyl rubber liner.
Anyone could give me some details or had similar experience?
Best Regards