koruma

Electrical
Dec 28, 2001
19
Hi
I need to butt-weld galvanized steel wire...does anybody knows how can I restore the zinc coat in the welded joint to its original specifications? the wire is ASTM B 498 galvanized steel wire.
 
Replies continue below

Recommended for you

They sell cans of spray on galvanizing that you can find in any welding or metal working magazine or possibly at Grainger or McMaster-Carr.

Not sure how well it works - but they have sold it for years!! I guess people keep buying it.

Welding galvanizing puts out some very nasty vapors - can't remember what - but know that precautions MUST be taken.

I am a strcutural....not welding engineer.
 