Does a butterfly valve for steam service need to have metal seats?
Design conditions:
Saturated steam, 200 psig and 400F
I'm looking at high-performance butterfly valves with the following specs:
carbon steel body (WCB), ANSI class 150 to B16.34 (200 psig, 400F)
Lug style
Not sure if I could use seats other than metal for these service conditions. I keep hearing soft seats won't survive the temperature.
Does anyone have experience with TFM (second generation polymer) seats?
Metal seated butterfly valves have long lead time.
I'd appreciate Any help, comments, recommendations and advice
Thanks in advance
Does a butterfly valve for steam service need to have metal seats?
Design conditions:
Saturated steam, 200 psig and 400F
I'm looking at high-performance butterfly valves with the following specs:
carbon steel body (WCB), ANSI class 150 to B16.34 (200 psig, 400F)
Lug style
Not sure if I could use seats other than metal for these service conditions. I keep hearing soft seats won't survive the temperature.
Does anyone have experience with TFM (second generation polymer) seats?
Metal seated butterfly valves have long lead time.
I'd appreciate Any help, comments, recommendations and advice
Thanks in advance