Can some body inform which is the BS or BS EN standard which gives the Electrode (SMAW) and SAW Flux and wires classification.

Thanks in advance
 
Here's a list extracted from the BSI website. Keywords welding consumables classification....

BS EN ISO 1071:2003 Welding consumables. Covered electrodes, wires, rods and tubular cored electrodes for fusion welding of cast iron. Classification. Current

BS EN ISO 14172:2003 Welding consumables. Covered electrodes for manual metal arc welding of nickel and nickel alloys. Classification. Current

BS EN ISO 18273:2004 Welding consumables. Wire electrodes, wires and rods for welding of aluminium and aluminium alloys. Classification. Current

BS EN ISO 18274:2004 Welding consumables. Solid wires, strips and rods for fusion welding of nickel and nickel alloys. Classification Current

BS EN 440:1995 Welding consumables. Wire electrodes and deposits for gas shielded metal arc welding of non alloy and fine grain steels. Classification Current

BS EN 499:1995 Welding consumables. Covered electrodes for manual metal arc welding of non alloy and fine grain steels. Classification Current

BS EN 756:2004 Welding consumables. Solid wires, solid wire-flux and tubular cored electrode-flux combinations for submerged arc welding of non alloy and fine grain steels. Classification Current

BS EN 757:1997 Welding consumables. Covered electrodes for manual metal arc welding of high strength steels. Classification Current.

BS EN 758:1997 Welding consumables. Tubular cored electrodes for metal arc welding with and without a gas shield of non-alloy and fine grain steels. Classification. Current, Confirmed

BS EN 1597-3:1997 Welding consumables. Test methods. Testing of positional capability of welding consumables in a fillet weld Current, Confirmed

BS EN 1599:1997 Welding consumables. Covered electrodes for manual metal arc welding of creep-resisting steels. Classification Current, Confirmed

BS EN 1600:1997 Welding consumables. Covered electrodes for manual metal arc welding of stainless and heat resisting steels. Classification Current, Confirmed

BS EN 12070:2000 Welding consumables. Wire electrodes, wires and rods for arc welding of creep-resisting steels. Classification Current

BS EN 12071:2000 Welding consumables. Tubular electrodes for gas shielded metal arc welding of creep-resisting steels. Classification. Current

BS EN 12072:2000 Welding consumables. Wire electrodes, wires and rods for arc welding of stainless and heat-resisting steels. Classification Current

BS EN 12073:2000 Welding consumables. Tubular cored electrodes for metal arc welding with or without a gas shield of stainless and heat-resisting steels. Classification.Current

BS EN 14295:2003 Welding consumables. Wire and tubular cored electrodes and electrode-flux combinations for submerged arc welding of high strength steels. Classification
Current

00/708210 DC Welding consumables. Welding consumables for fusion welding of cast iron. Classification (ISO/DIS 1071). Current, Draft for Public Comment

03/102141 DC BS EN 14640. Welding consumables. Solid wires and rods for fusion welding of copper and copper alloys. Classification Current, Draft for Public Comment

03/107142 DC EN 14700. Welding consumables. Welding consumables for hard-facing Current, Draft for Public Comment

BS 639:1976 Specification. Covered electrodes for the manual metal-arc welding of carbon and carbon manganese steels Withdrawn, Revised

BS 639:1986 Specification for covered carbon and carbon manganese steel electrodes for manual metal-arc welding Withdrawn, Superseded

BS 5465:1977 Specification for electrode wires and fluxes for the submerged arc welding of austenitic stainless steels based on weld metal composition Withdrawn, Revised

BS 5465:1987 Specification for electrodes and fluxes for the submerged arc welding of austenitic stainless steels Withdrawn, Superseded

BS 7084:1989 Specification for carbon and carbon-manganese steel tubular cored welding electrodes Withdrawn, Revised

BS EN 756:1996 Welding consumables. Wire electrodes and wire-flux combinations for submerged arc welding of non alloy and fine grain steels. Classification. Withdrawn, Revised.

Hope this is useful.

Andy

 