BS-B23

Status
Not open for further replies.

steinjanssens

New member
Joined
Aug 11, 2005
Messages
2
Location
BE
Hi,

I'm looking for compression allowables for the Al-Bronze material BS-B23.

Thanks,
Stein Janssens
M&P engineer
 
steinjanssens...

Do You mean???

BRITISH STANDARD BS B 23:1991
Specification for
Copper-aluminium nickel-iron alloy rods, sections, forging stock and forgings

If so, spec is available thru IHS [Information Handling Systems]. NOTE: proprietary markings on IHS forbid copying and sending it to You... and there too many different data tables to extract.

Regards, Wil Taylor
 
Thanks Wil,

I got plenty of specs but never compression ultimate values on it. Probably because the compression ultimate failure criteria is arbitrary and differs sometimes. Anyway, there must be somewhere compression ultimate allowables/values on this planet..

Thanks for your reaction,
Stein
 