Tmoose
Mechanical
- Apr 12, 2003
- 5,636
Got some danged castings made of hi chrome cast iron that keep provoking questions. One is justification of acceptance criteria for linear indications/heat checks/cracks.
I've made some decent models and used two different general purpose FEA programs to solve for max principal (tensile) stress as appropriate to determine "hot" locations and perilous orientations for what is essentially static loading.
I'll be making a few trial FEA runs with synthetic cracks, but expect realistically sharp crack geometry will just trigger a bunch of singularity warnings, as they should.
Fracture mechanics has been suggested as the necessary tool to determine acceptable indication size limits when oriented "badly."
So, now I'm starting at the very beginning independently learning about fracture mechanics.
One dilemma I have is that the "length" of actual indications is all we are going to have to work with. I think I know about how deep they are likely to be, so could make some reasonable ASSumptions there. Useful/necessary Material properties are pretty much nonexistent.
Does anyone have some hints to help ease this process ?
I've made some decent models and used two different general purpose FEA programs to solve for max principal (tensile) stress as appropriate to determine "hot" locations and perilous orientations for what is essentially static loading.
I'll be making a few trial FEA runs with synthetic cracks, but expect realistically sharp crack geometry will just trigger a bunch of singularity warnings, as they should.
Fracture mechanics has been suggested as the necessary tool to determine acceptable indication size limits when oriented "badly."
So, now I'm starting at the very beginning independently learning about fracture mechanics.
One dilemma I have is that the "length" of actual indications is all we are going to have to work with. I think I know about how deep they are likely to be, so could make some reasonable ASSumptions there. Useful/necessary Material properties are pretty much nonexistent.
Does anyone have some hints to help ease this process ?