qualitypro
Mechanical
We had brazed some production joints in the Instrument air system before we realised that our personnel have to be qualified as per Sec IX. Subsequently, we qualified our brazers and continued our production. We performed a pneumatic test as per B31.1 and the system passed the leak test at about 182 psig. My client does not accept the leak test performed and insists that destructive testing needs to be carried out on the first braze joint of each brazer prior to his performance qualification.
Is there any provision in either of the codes to accept the subject system as is?