I recently ordered Rockwell B standards and (I should have known in advance) received brass, which for the Microdur MIC-10 I use is out of the question. (I'd like to know in general how brass started to be used for calibration blocks.)
I'd like to hear people's experiences and solutions to Microdur's requirement (in their operating manual) that calibration blocks be of 'similar material' to that being tested. By 'similar material' do they merely mean similar elastic (Young's) modulus? I am looking at testing the entire range of Cr-Mo steels up to 10% Cr, including some exotic CSEF alloys.
I'd like to hear people's experiences and solutions to Microdur's requirement (in their operating manual) that calibration blocks be of 'similar material' to that being tested. By 'similar material' do they merely mean similar elastic (Young's) modulus? I am looking at testing the entire range of Cr-Mo steels up to 10% Cr, including some exotic CSEF alloys.