I'm making a brass table for a beautician's salon. The customer wants it to look satin finish. Is there any thing that can be put on that will make the brass stay the finish we make, with out it oxidizing or discolouring. The people use acetone so clear lacquer will not work, looked all over and it seem only solution is to keep using brasso or something similar