Mar 14, 2022 #1 RazaR Mechanical Joined Mar 14, 2022 Messages 1 Location IN Hello everyone, There are some brass sheets available in markets of 1 mm thk and 2 mm thk in grade C27400. Can i get ASTM standard for the same to cross verify mechanical properties of the sheet for that grade?
Hello everyone, There are some brass sheets available in markets of 1 mm thk and 2 mm thk in grade C27400. Can i get ASTM standard for the same to cross verify mechanical properties of the sheet for that grade?
Mar 14, 2022 #2 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA google problems? https://alloys.copper.org/alloy/C27400Just make sure that you know the temper, is it hard rolled? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
google problems? https://alloys.copper.org/alloy/C27400Just make sure that you know the temper, is it hard rolled? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed