I have an aluminum AN832-3D (bulkhead union, two male 3/8-24 UNF w/ 37° flares). I need to connect it to a brass male 1/8 NPT fitting and can't seem to find a female/female fitting-coupling that will do the trick.
 
Replies continue below

Recommended for you

If it is not aircraft use you could try these people. or if it is an aircraft part You may have to use a larger pipe thead and an adaptor to get down to the size you need.
B.E.



The good engineer does not need to memorize every formula; he just needs to know where he can find them when he needs them. Old professor
 
I checked aircraft spruce they don't appear to have what i need. The existing connections are both male so I need to find a double female fitting.
 
iongno--you should be aware that coupling brass to aluminum is never a good plan because of the potential for galvanic corrosion.
 
You might try googling "Autoclave Engineering".

I agree with the caveat about galvanic corrosion. Are there aluminum connections on the other side of the bulkhead union? Any chance of changing the bulkhead fitting to a more compatible metal?
 
Berkshire - Earl's Ano Tuff may do the trick. Ideally I would like to have just one part to make the connection. This part would be great, if only it was an AN-3 and at $37 is more than I would like to spend.

swall - I agree corrosion is a concern. However the BH fitting attaches to an aluminum channel. The BH fitting is a lot cheaper and easier to replace than the Al channel. The treads will have ARP thread sealer added that should help with corrosion.

The brass fitting is existing hardware for 1/8” copper tube brake lines. Replacing the lines is out of the question. The system I’m designing is a kit. I would like to keep the fittings so the end user does not need special tools to change it and can go back to original equipment.
 
Mint

I have added your link to my favorites . That is a very useful site.
And I have given you a star for it.