May 4, 2022 #1 tmgczb Structural Joined May 12, 2021 Messages 176 Location CN As the title, I know that if it is painted, the friction coefficient would be changed, thus shear resistance of base plate would be reduced. But I didn't find any description in any codes or standards.
As the title, I know that if it is painted, the friction coefficient would be changed, thus shear resistance of base plate would be reduced. But I didn't find any description in any codes or standards.
May 5, 2022 #2 JLNJ Structural Joined Oct 26, 2006 Messages 1,986 Location US Normally shear is taken directly through side-bearing on an anchor rod or through a shear key. The paint or lack of it on the bottom of a base plate makes no difference as to the shear capacity. Upvote 0 Downvote