Bonding TPU compnents together

Status
Not open for further replies.

craigmj

Mechanical
Joined
Feb 5, 2006
Messages
37
Location
US
I'm looking for an agressive one part bonding agent for injection molded TPU materials (90 Shore A).

Here is an example:

Id like to find something that does not require UV light to activate, and is assembly line friendly (non-toxic).

What about primers?

Thanks
Craig
 
HB Fuller has TPU primers and adhesive, which are solvent base or water-based , or HMMC - hotmelt moisture cure.
Normally these primer donot need a UV to active.
an EVA primer normally need that.
DongSung also has TPU primer and adhesive, such TPU (90 shoreA) using as outsole.
 