What the effective adhesives for bonding 5052 Al sheet 1mm thick to mild steel shs with a room temp cure. So far adhesives have focused on the usual Sikaflex products and some Epoxy resins. Has anyone got experience of structural acrylics for such a purpose? Mechanical fixing will also be used with the used of monel metal rivets to assist with peel performance.
 
Replies continue below

Recommended for you

I need to adhere 5052 Al honeycomb panel to 400-450 dual grade Mpa mild steel for motorsport applications.
 