how can i bond polystyrene midsole with rubber sole using polyurethane solvent based adhesive system.
the process is:
clean polystirene with MEK, Apply promoter adhesion (i dont know wich one) and cementing with PU adhesive.

any tip???
Thanks
 
How about telling us what you have done already that didn't work?



Mike Halloran
Pembroke Pines, FL, USA
 
I tried with this adhesion promotors after clean with MEK:
1.chlorinated polyolefines at 6% pbw in MEK/TOL
2.Desmodur L-1260 (isocyanate)at 5% in ETHYL ACETATE
3. Hypalon CP-337 at 6% in MEK/TOL/CICLOHEXANONE

all the results were adhesion fail over the PS. The PU solvent based adhesive did not attach over the surface of the polystyrene
 