Mar 19, 2004 #1 iqramirez Chemical Joined Mar 16, 2004 Messages 5 Location MX hello all, i am working in shoe industry, and i have many problems for bonding nylon, i made a primer using phenol in solution in Ehthyl acetate, but the results presents parts with adhesion fail. any suggestion? thanks
hello all, i am working in shoe industry, and i have many problems for bonding nylon, i made a primer using phenol in solution in Ehthyl acetate, but the results presents parts with adhesion fail. any suggestion? thanks