I have an application where I have a number of cast iron rods which have fractured. I would like to bond these back together. They are not carrying any significant loads. Is there any way of bonding cast iron that is successful?

---------------------------------------------------------------------------------------------------------------------
[pimp]

"The world keeps turning, it keeps me in my place; where I stand is only three miles from space"
Spiritualized
 
Replies continue below

Recommended for you

It is cheaper to get them recast,rather attempt to join by brazing .