It depends on which grade of stainless steel, whether it is cold worked or not, and the diameter of the bolt. Check ASCE 8-02 for guidance.
As for your A304 bolts, for hot finished bolts, the nominal tensile is 56ksi, shear 33.7ksi (threads in shear plane) or 45ksi (threads not in shear plane)...ref. Table 6, ASCE 8-02.
If cold worked, the nominal stress goes up slightly, but depends on the diameter of the bolt.