SteelMover
Structural
I have a pretensioned bolted connection that always sees a rather high level of vibration where I want to use loctite thread locker to prevent bolt rotation, not safety wire. Does anyone have a clever & durable way of marking the bolts for inspection to determine whether or not there has been any unwanted rotation?
In the past I have ground a thin match line into the bolt head and steel using an abrasive wheel or provided match marks with paint.
Are there any less expensive options other than safety wire that you know of that ENSURE the bolts are not rotating?
Thanks!
In the past I have ground a thin match line into the bolt head and steel using an abrasive wheel or provided match marks with paint.
Are there any less expensive options other than safety wire that you know of that ENSURE the bolts are not rotating?
Thanks!