Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Bolt head "letter" identification

Status
Not open for further replies.

tmcgett

Electrical
Joined
Jan 3, 2004
Messages
13
Looking for info on a grade 8 ( 1" shaft dia. ) with the letters "BY" on center of head. What's the BY stand for?

Also this bolt was used instead of a required grade 10.9
( 27mm / 1" 1/8 shaft dia. ) on a critical structure.

What magnitude of danger if any would this pose ?

Thanks
 
If it says 8.8 on the bolt head then its an ISO bolt. The BY could be a manufacturers marking

Difference between 8.8 and 10.9 is significant

proof load (psi) 85000 vs 120000
min yield strength (psi) 92,000 vs 130000
min Tensile Strength (psi) 120000 vs 150000

The danger depends on the application, but if it calls for a 10.9 then it should be a 10.9
 